The disadvantages of using internally chromium plated cylinder liners.
| Identifier | ExFiles\Box 127\3\ scan0114 | |
| Date | 5th October 1936 | |
| EXPERIMENTAL DEPARTMENT REPORT. REFERENCE :- Hs {Lord Ernest Hives - Chair} /Wd. {Mr Wood / Mr Whitehead} 7/WJ.8.10.36. Subject of Report :- An internally chromium plated cylinder liner. General Conclusion :- The use of liners chromium plated in the bore has disadvantages without any compensating advantages. Copies of Report Circulated to :- Hs. {Lord Ernest Hives - Chair} E. {Mr Elliott - Chief Engineer} By. {R.W. Bailey - Chief Engineer} Rg. {Mr Rowledge} RHC. {R. H. Coverley - Production Engineer} Db. {Donald Bastow - Suspensions} Report to be noted for further action by :- Test carried out on :- Universal Single Cylinder Unit. By :- F.C.E. Test No. Date :- 5.10.36. RR 2X (50H) (84267. 21-6-35) G.C.B. | ||
From the Rolls-Royce experimental archive: a quarter of a million communications from Rolls-Royce, 1906 to 1960's. Documents from the Sir Henry Royce Memorial Foundation (SHRMF).