Letter detailing the heat treatment process for an S.82 axle shaft.
| Identifier | ExFiles\Box 114\1\ scan0114 | |
| Date | 17th September 1937 | |
| 1015. Rm {William Robotham - Chief Engineer} 4/Gry {Shadwell Grylls} /R. 17th Sept., 1937. P. Berthon, Esq., English Racing Automobiles Ltd., BOURNE, Lincs: Dear Berthon, With regard to your telephone query about the heat treating of S.82 axle shaft, this should consist of:- heat to 820°C and quench in oil " " 760°C " " " brinell test of both ends of the shaft 360 to 400. In our size of furnace we heat the Bentley axle shafts for 35 minutes, 25 minutes of which is bringing them up to the temperature, and 10 minutes soaking at that temperature. This may not necessarily apply to the E.N.V. furnace, and it will not do any harm if they remain at that temperature for more than 10 minutes. At a brinell of 400 the material can just be machined, although it is rather difficult. In our case we machine the splines after the heat treatment. I am getting one of our people to write to you about valve stelliting, which I hope will get you out of your difficulty. Yours sincerely, | ||
From the Rolls-Royce experimental archive: a quarter of a million communications from Rolls-Royce, 1906 to 1960's. Documents from the Sir Henry Royce Memorial Foundation (SHRMF).