Rolls-Royce Archives
         « Prev  Box Series  Next »        

From the Rolls-Royce experimental archive: a quarter of a million communications from Rolls-Royce, 1906 to 1960's. Documents from the Sir Henry Royce Memorial Foundation (SHRMF).
Graph of terminal potential difference vs. rate of charge for Paragon and Exide 6-volt batteries at various temperatures.

Identifier  ExFiles\Box 168b\3\  img075
Date  19th June 1930
  
TERMINAL P.D.
RATE OF CHARGE (AMPERES)
CURVES OF THE SUSTAINED P.D. ON A
6 VOLT 'PARAGON' BATTERY AND A
6 VOLT 'EXIDE' 3MRB-12EL BATTERY
TAKEN AT VARIOUS RATES OF CHARGE
WITH A FIXED TEMPERATURE & THE
BATTERY IN A FULLY CHARGED CONDITION

Curve Labels:
PAR 4°C 39°F
EXIDE 4°C 39°F
PAR 11°C 52°F
EXIDE 11°C 52°F
PAR 14°C 58°F
EXIDE 14°C 58°F
PAR 15.5°C 60°F
EXIDE 15.5°C 60°F
H.J.S / 19.6.30
  
  