Test results table for wear and performance of different material linings under various conditions.
| Identifier | ExFiles\Box 103\1\ scan0096 | |
| Date | 3rd May 1934 | |
| -4- Ha/FJH. {Fred J. Hardy - Chief Dev. Engineer} 20/RW. 3.5.34. Type of lining Wear due to 200 2000-3000 r.p.m. slips. Additional slips 500-3000 to produce total wear of 0.100" Remarks. RAD.11 2 hrs. at 700°F. {Mr Friese} 0.006 - Behaved perfectly throughout 2000-3000 slips and first 4 of 500-3000 slips. Slipped and smoked from 4th to 40th of 500-3000 slips. No improvement over 1 hr. at 700°F. {Mr Friese} Test discontinued. RAD.11 1.5 hrs. at 800°F. {Mr Friese} 0.008 250 Behaved perfectly throughout 2000-3000 slips and first 28 of 500-3000 slips. Slipped and smoked at 29th, 30th 38th, 39th and 50th of 500-3000 slips. RAD.5 1.5 hrs. at 600°F. {Mr Friese} 0.004 - Very bad slipping and smoking throughout 2000-3000 slips and first 50 of 500-3000 slips. Test discontinued RAD.11 chemically treated by Ferodos. 0.005 355 Behaved perfectly throughout 2000-3000 slips. Had slipping but no smoke for first 20 500-3000 slips and at approx. every 7th slip up to 90. From 90 onwards clutch behaved perfectly. | ||
From the Rolls-Royce experimental archive: a quarter of a million communications from Rolls-Royce, 1906 to 1960's. Documents from the Sir Henry Royce Memorial Foundation (SHRMF).