Sourcing and testing an American alloy for use in Bentley steel bearing shells.
| Identifier | ExFiles\Box 115\1\ scan0166 | |
| Date | 4th December 1936 | |
| Handwritten top: If the Hoyt high lead alloy shows any promise we might try one below. Rm {William Robotham - Chief Engineer} Typed: To Hl.(Laboratory) from Rm {William Robotham - Chief Engineer} 1020 We want to obtain some bearings in the American alloy which is known as 14.B. Its' composition it - 5% tin. 15% antimony. 80% lead. Will you please let us know where we can obtain sufficient quantity to line one set of Bentley steel bearing shells, and also whether a 70 lead 30 tin solder will give good adhesion. Handwritten bottom: Rm {William Robotham - Chief Engineer} Please order from Fdy. High lead alloys are generally more difficult from adhesion standpoint. Rm {William Robotham - Chief Engineer} This alloy much softer than RR whitemetal. will try 70/30 first. HS {Lord Ernest Hives - Chair} | ||
From the Rolls-Royce experimental archive: a quarter of a million communications from Rolls-Royce, 1906 to 1960's. Documents from the Sir Henry Royce Memorial Foundation (SHRMF).