And diagrams detailing an experiment on the contact resistance of oxidised tungsten points.
| Identifier | ExFiles\Box 35\5\ scan 141 | |
| Date | 24th January 1919 | |
| RR 300 (120B) (SF 349 24-1-19) MP 200552 88215 ROLLS-ROYCE LIMITED. INSTRUCTIONS. To: Oxidation of Tungsten Points (cont'd) 19 Order No: Customer's No.: 2 Re: darker spots. The contact resistance was now observed, by passing a current from a 2 volt battery & through a carbon resistance. The following results were noted. Current with rods short-circuited 10 amps. With sides placed together 9.8 - 10 amps. With faces together 7.5 to 8.0 amps. Positive face to negative side, 7.5 - 8.0 amps. Negative face, to positive side 9.8 amps. (Cont'd 2) Signed This Sheet must be filed on completion of the work. | ||